通化硕抠家具有限公司

    螺紋過盈量對特殊螺紋接頭性能的影響

    Influence by Thread Interference on Premium Connection Performance

    • 摘要: 運用ABAQUS軟件計算了在上扣、上扣+拉伸條件下Φ139.70 mm×9.17 mm規(guī)格P110鋼級特殊螺紋不同螺紋過盈量對接頭性能的影響。模擬結果表明:上扣后,當螺紋過盈量∧0.159 0 mm時,密封面處接觸壓力變化不大;當螺紋過盈量∧0.238 5 mm時,隨著螺紋過盈量的增加,密封面接觸壓力下降明顯。上扣+拉伸條件下,隨著螺紋過盈量的增加,密封面接觸壓力下降,同時接觸位置向臺肩處移動;當螺紋過盈量∧0.079 5 mm時,拉伸失效斷裂在螺紋處;當螺紋過盈量∧0.159 0 mm時,拉伸失效斷裂在管體。

       

      Abstract: Analyzed is the influence by different interferences of the Φ139.70 mm×9.17 mm P110 premium thread on the connection performance by means of the ABAQUS software,and under conditions of make-up,and make-up plus tensile loading. Result from the simulation reveals that if,after make-up,the thread interference is more than 0.159 0 mm,the contact pressure on the sealing surface changes a little;if the thread interference is more than 0.238 5 mm,along with increase of the interference,the contact pressure of the sealing surface is going down remarkably;under the condition of make-up plus tensile loading,along with increase of the interference,the contact pressure of the sealing surface is decreased,while the contact position is shifted towards the shoulder;and when the interference is more than 0.079 5 mm,tensile failure fracture takes places at the thread section,while when the interference is more than 0.159 0 mm,the similar fracture takes places with pipe body.

       

    /

    返回文章
    返回