    J55套管射孔開(kāi)裂分析

    INVESTIGATION OF PERFORATION CRACKING OF J55 CASING

    • 摘要: 詳細(xì)分析了新日鐵生產(chǎn)的J55套管的化學(xué)成分、機(jī)械性能及金相組織,指出由于化學(xué)成分設(shè)計(jì)不合理以及熱軋工藝不當(dāng)所造成的晶粒粗大、組織不良等是引起套管韌性低劣并導(dǎo)致射孔開(kāi)裂的主要原因。同時(shí)還應(yīng)用射孔安全韌性判據(jù)的研究成果,論證了該J55套管射孔開(kāi)裂的必然性。

       

      Abstract: Based on detail analysis of the chemical composition, mechanical properties and metallographic structure of the J55 casing made by Nippon Steel Corp.,Japan,it is concluded that the major causes responsible for the poor toughness and perforation cracking of the said casing areinappropriately designed chemical composition and coarse gains and poor structure due to inadequate hot-rolling process. Also discussed is the inevitability of the said J55 casing perforation cracking on the basis of result from research concerning perforation safe toughness.

       

    /