    • 摘要: 介紹了國內(nèi)外核電主管道制造技術(shù)的發(fā)展;指出目前國內(nèi)制造第三代核電主管道的方法是采用實心電渣重熔坯鍛造,再通過機(jī)加工掏空方式成型主管道的內(nèi)孔;針對主管道制造傳統(tǒng)工藝存在材料利用率低、生產(chǎn)周期長以及質(zhì)量不穩(wěn)定等特點,探討了工藝改進(jìn)的方向。分析認(rèn)為:以離心鑄造空心錠或電渣重熔空心錠為坯料的空心鍛造工藝將最終替代目前的實心鍛造工藝。

       

      Abstract: Described in the essay is the developments concerning the manufacture technologies for the nuclear power reactor coolant pipe as made both at home and abroad.It is pointed out that at present the process as used at home for making the third generation coolant pipe is first forging the solid electroslag remelting ingot,and then boring the shaped piece with mechanical method.Addressing the disadvantages concerning the conventional manufacturing process for the coolant pipe,i.e.,poor material utilization rate,rather long production cycle and product quality inconsistency,etc.,the orientation of technological improvement is discussed.The result of relevant analysis leads to such a forecast that the hollow forging process using the centrifugally-cast hollow ingot or the electroslag remelting hollow ingot as the blank will eventually replace the currently-employed solid billet forging process.

       

    /

    返回文章
    返回