    • 摘要: Assel軋管機生產薄壁無縫鋼管(徑壁比≥25)時,存在著荒管頭部易產生喇叭口,軋制過程中荒管甩動大,內表面易產生內螺紋缺陷等問題,嚴重制約著機組產能的釋放。湖北新冶鋼有限公司通過采用增設軋管機后臺導衛(wèi)裝置及前臺檢測裝置,改進軋管機輥型,優(yōu)化軋制工藝參數等措施,大大減少了軋制過程中軋扭、卡鋼事故的發(fā)生,軋制的薄壁無縫鋼管內螺紋缺陷也明顯減輕,壁厚精度達到±8%,成材率在90%以上。

       

      Abstract: In case of rolling light-wall seamless steel tubes with D/S ≥25 with the Assel mill, several problems are apt to be encountered with, including forming of bell-like end of the shell, strenuously swinging of the shell during rolling, and developing of defective inner surface spiral mark and so on, which greatly impede fully tapping of the operation line’ s production capacity. Accordingly, a series of technical modification actions are taken by Hubei Xinyegang Steel Co., Ltd., including adding a guiding device to the run-out table and relevant measuring units to the incoming section, improving the roll profile of the mill and optimizing the rolling process parameters, etc. As a result, failures as occurring in the rolling operation like material twisting or jamming are considerably reduced, and the severity of the said inner surface spiral mark is so lessened, while the tube wall thickness tolerance is tightened up to ±8%, and the mill yield increased to over 90%.

       

    /

    返回文章
    返回